Sell Offers
Sintering methord : WC (Co 8%)
Density(g/cm3): 14.5 – 14.9
Bending strength (MPa) :1750
Hardness(HRA): 90
Thermal expansion coefficient (10-6/℃) :5.2
Sintering methord : WC (Ni 6%)
Density(g/cm3): 14.5 – 14.9
Bending strength (MPa) :1550
Hardness(HRA):88
Thermal expansion coefficient (10-6/℃) : 4.2